Samsung Galaxy S25 Edge Durability Test
• The Galaxy S25 Edge, known for its ultra-thin 5.8mm profile and premium design, underwent durability tests.
• Despite using Corning's Gorilla Glass Ceramic 2 and Gorilla Glass Victus 2, the front screen cracked upon impact, indicating the phone's fragility.
• The phone's structural durability was mixed, with the titanium frame withstanding significant pressure without breaking. However, a slight panel gap appeared near the power button.
• The device's screen began showing scratches at level 6 on the Mohs hardness scale, with deeper grooves at level 7, which is standard for flagship smartphones.
• The device's glass panels are susceptible to cracking upon impact, recommending the use of a robust protective case.
• The test results can be viewed in various videos.